UNS C70600 Wire
Cupronickel alloys are widely used for marine applications due to their excellent resistance to seawater corrosion, low biofouling rates, and good fabricability.
CALL US:
1-866-725-8609Cupronickel alloys are widely used for marine applications due to their excellent resistance to seawater corrosion, low biofouling rates, and good fabricability.
Cupronickels Alloys: Condensers; Evaporator and heat exchanger application; Ferrules; Applications where biofouling is a concern; Silver colored coinage.
Copper-Nickel-Tin Alloys: Relay springs; Switch springs; Lead frames; Telecommunication connectors
Cupronickel alloys are widely used for marine applications due to their excellent resistance to seawater corrosion, low biofouling rates, and good fabricability. They have provided reliable service for decades while offering effective solutions to today's technological challenges addition of nickel to copper improves strength and corrosion resistance while allowing the alloy to remain ductile.
Alloy C72500: Developed by Bell Laboratories to solve issues of stress corrosion found in field parts. The alloy blends the strength of Phosphor Bronze and the Corrosion resistance of Nickel Silver without too much loss of electrical conductivity. A combination of very good fatigue strength and resistance to corrosion and tarnish have also made this alloy an excellent choice for other applications found in corrosive
C70600 Balance 9.0-10.0* 0.05 max 1.0-1.8 1.0 max 1.0 Mn max
C71500 Balance* 29.0-33.0 0.05 max 0.40-1.0 max 1.0 max 1.0 Mn max
C71200 Balance 8.5-10.5* 0.05 max 0.6 max 0.50 max 1.8-2.8 Sn,
0.20 Mn max
* Contact Ulbrich Wire for request regarding the availability of other copper alloys.
* Contact Ulbrich Technical Department for limits for additional trace elements and impurity levels.
* Copper plus sum of named elements 99.5% min.
* Nickel Values include Cobalt.
* Copper Values include Silver.
Physical Properties
Typical Density: 0.321 - 0.323 lbs/in3, 8.88 - 8.94 g/cm3
Electrical Conductivity: (% IACS at 68° F 20°C, annealed): 4.6 - 11 %
Mean Coefficient of Thermal Expansion: µin/in-° F:
68 - 572 ° F: 8.5 - 9.2
Thermal Conductivity: BTU-in/hr-ft2-° F at 68 ° F: 17 - 31
Modulus of Elasticity: KSI
18 - 22 x 103 in tension
Profile, Round, Flat, Square
Ultimate Tensile Strength: 43 KSI min (296 MPa min)
Yield Strength: 19 KSI min (131 MPa min)
Elongation: 35% min
These alloys can be cold worked to various tempers.
* Actual physical and mechanical properties are alloy dependent. Contact Ulbrich Technical Service for alloy specific properties.
Contact Ulbrich Wire for specific information.
XC - Extra clean. Annealed or annealed and cold rolled. Contact Ulbrich Wire with special finish requests.
These alloys are non hardenable by heat treatment.
Contact Ulbrich Wire for specific information.
Limitation of Liability and Disclaimer of Warranty: In no event will Ulbrich Stainless Steels & Special Metals, Inc., be liable for any damages arising from the use of the information included in this document or that it is suitable for the 'applications' noted. We believe the information and data provided to be accurate to the best of our knowledge but, all data is considered typical values only. It is intended for reference and general information and not recommended for specification, design or engineering purposes. Ulbrich assumes no implied or express warranty in regard to the creation or accuracy of the data provided in this document.
Thanks for your interest in Ulbrich! Whether you're developing a new product or ramping up production, we'll be happy to learn more about your specific needs. Please fill out the form below, and we will promptly get back to you with a quote or, if needed, a request for more information.