UNS C10500 Wire

In general, copper alloys exhibit good to excellent corrosion resistance and high thermal conductivity and very high electrical conductivity.

Full Name
Email
Company
Business Address

Flat, Shaped and Round Wire
ASTM B152, ASTM B747, QQ-C-576

Applications

Electrical/electronic and solar applications where strength is not required. Additional applications are downspouts, gutters, roofing, gaskets, heat sinks, busbars, nails, printing rolls, rivets, etc. parts.

Description

In general, copper alloys exhibit good to excellent corrosion resistance and high thermal conductivity and very high electrical conductivity. Pure copper's electrical conductivity is so high that many metals are measured against it in the form of the IACS (International Annealed Copper Standard).

Chemistry Typical

UNS# COPPER* OXYGEN SILVER PHOSPHORUS ARSENIC

C10100 99.99 min 0.0005 max 0.0005 max

C10200 99.95 min 0.001 max 0.0003 max

C10400 99.95 min 0.001 max 0.027 min

C10500 99.95 min 0.001 max 0.034 min

C10700 99.95 min 0.001 max 0.085 min

C11000 99.90 min

C12000 99.90 min 0.004-0.012

C12100 99.90 min 0.014 0.004-0.012

C15000 Balance* 0.10-0.20 Zr

C15500 99.75 min 0.027-0.10 0 .040-0 .080 | 0.08-0.13 Mg

* Contact Ulbrich Wire for request regarding the availability of other copper alloys.
* Contact Ulbrich Technical Department for limits for additional trace elements and impurity levels.
* Copper Values include Silver.
* Copper plus named elements.

Physical Properties


Typical Density: 0.332 lbs/in3, 8.92 g/cm3


Electrical Conductivity:(% IACS at 68° F 20°C, annealed): 85-101%


Specific Heat: BTU/lb-° F (J/g-°C): 0.0920 (0.385)


Mean Coefficient of Thermal Expansion: µin/in-° F (µm/m-°C)
68 - 572 °F (20 - 300 °C): 9.8 (17.6)


Thermal Conductivity: BTU-in/hr-ft2-° F (W/m•K): 2712 (390.8)


Modulus of Elasticity: KSI (MPa) 17 x 103 in tension

Melting Range: 1981 °F (1083 °C)

Forms


Profile, Round, Flat, Square


Mechanical Properties at Room Temperature


Properties: Annealed Typical

Ultimate Tensile Strength: 26 - 38 KSI (179 - 262 MPa)

Yield Strength: 10 KSI (69 MPa) Nominal

Elongation: 35%

Properties: Tempered

Copper alloys can be cold worked to various tempers.

*Actual physical and mechanical properties are alloy dependent. Contact Ulbrich Technical Service for alloy specific properties.

Additional Properties

Corrosion Resistance

Contact Ulbrich Wire for specific information.

Wire Finishes

XC - Extra clean. Annealed or annealed and cold rolled. Contact Ulbrich Wire with special finish requests.

Heat Treatment

Copper alloys are non hardenable by heat treatment.

Welding

Contact Ulbrich Wire for specific information.

Limitation of Liability and Disclaimer of Warranty: In no event will Ulbrich Stainless Steels & Special Metals, Inc., be liable for any damages arising from the use of the information included in this document or that it is suitable for the 'applications' noted. We believe the information and data provided to be accurate to the best of our knowledge but, all data is considered typical values only. It is intended for reference and general information and not recommended for specification, design or engineering purposes. Ulbrich assumes no implied or express warranty in regard to the creation or accuracy of the data provided in this document.

Get a Quote

Thanks for your interest in Ulbrich! Whether you're developing a new product or ramping up production, we'll be happy to learn more about your specific needs. Please fill out the form below, and we will promptly get back to you with a quote or, if needed, a request for more information.

  • Product

  • Contact information

  • Request Details

  • Additional criteria and file

Success

Success!

Thank you!

Form submitted successfully. Someone from Ulbrich will be in-touch with you soon.

GETTING STARTED

Which product or service are you interested in?

To ensure your request gets routed to the right Ulbrich team, let us know which
metal product, or service you're looking to source.