Titanium Beta 21S Grade 21 Wire UNS R58210

Titanium Beta 21S offers the good cold formability and weldability of a beta strip alloy with greatly improved oxidation resistance and creep strength.

Full Name
Email
Company
Business Address

Titanium Beta 21S Shaped, Flat, Square, Round, Fine Wire, Plated and Un-plated ASTM B265

Titanium Beta 21S Wire Description


With high strength Titanium Beta 21 S (Timetal 21S) is a heat treatable, metastable titanium alloy developed as an oxidation-resistant, aerospace material and as a matrix for metal-matrix composites. Beta 21S offers the good formability and weldability of a beta alloy, but with greatly improved oxidation resistance and creep strength.

Applications

Chemistry Typical


Titanium: Balance
Molybdenum: 14.0-16.0
Niobium: 2.4-3.2
Aluminum: 2.5-3.5
Silicon: 0.15-0.25
Iron: 0.40 max
Oxygen: 0.11-0.17
Carbon: 0.05 max
Nitrogen: 0.05 max
Hydrogen: 0.015 max
Residuals each 0.10 max, total 0.40 max

Common Titanium Grade Names

Name

Code

Description 1Description 2ASTMAMSUNS
Titanium 21STI21SMetastable beta alloyTimetal 21SR58210

Physical Properties of Ti 21S


Density: 0.178 lbs/in³, 4.94 g/cm³

Mean Coefficient of Thermal Expansion: in/in/°F (mm/m/°C):
70-212°F (20-100°C): 3.93 x 10 (7.07)

Thermal Conductivity: BTU-in/h-ft-°F (W/m-°K): At 70°F
(21°C): 52.7 (7.6)

Modulus of Elasticity: KSI (MPa)
10.5-12 x 10³ (72-85 x 10³) in tension

Melting Point: 3034°F (1668°C)

Mechanical Properties at Room Temperature


Properties: Annealed (1550°F)


Ultimate Tensile Strength: 155 KSI min (1068 MPa min)
Yield Strength (0.2% offset): 110 KSI min (758 MPa min)
Elongation: 12%

Aged Properties: Typical


Aging Temp/Time: 1000°F / 8 HOURS
Ultimate Tensile Strength: 170 KSI min (1172 MPa min)
Yield Strength (0.2% offset): 160 KSI min (1103 MPa min)
Elongation: 4%

Aging Temp/Time: 1100°F / 8 HOURS
Ultimate Tensile Strength: 150 KSI min (1034 MPa min)
Yield Strength (0.2% offset): 140 KSI min (965 MPa min)
Elongation: 6%

Aging Temp/Time: 1275°F / 8 HOURS
Ultimate Tensile Strength: 125 KSI min (862 MPa min)
Yield Strength (0.2% offset): 115 KSI min (793 MPa min)
Elongation: 10%

Properties Tempered


Titanium Beta 21S can be cold rolled to achieve the temper properties required by specific customers and/or manufacturing requirements. Contact Ulbrich Wire for details.

Additional Properties


Corrosion Resistance


Refer to NACE (National Association of Corrosion Engineers) for recommendations.

Finishes


Inquire with Ulbrich Wire

Heat Treatment


Titanium Beta 21S can be hardened by aging

Welding


For best results refer to: SSINA’s “Welding of Stainless Steels and Other Joining Methods”

Limitation of Liability and Disclaimer of Warranty: In no event will Ulbrich Stainless Steels and Special Metals, Inc., be liable for any damages arising from the use of the information included in this document or that it is suitable for the ‘applications’ noted. We believe the information and data provided to be accurate to the best of our knowledge but, all data is considered typical values only. It is intended for reference and general information and not recommended for specification, design or engineering purposes. Ulbrich assumes no implied or express warranty in regard to the creation or accuracy of the data provided in this document.

Get a Quote

Thanks for your interest in Ulbrich! Whether you're developing a new product or ramping up production, we'll be happy to learn more about your specific needs. Please fill out the form below, and we will promptly get back to you with a quote or, if needed, a request for more information.

  • Product

  • Contact information

  • Request Details

  • Additional criteria and file

Success

Success!

Thank you!

Form submitted successfully. Someone from Ulbrich will be in-touch with you soon.

GETTING STARTED

Which product or service are you interested in?

To ensure your request gets routed to the right Ulbrich team, let us know which
metal product, or service you're looking to source.