Hastelloy® C4 (Alloy C-4) Wire UNS N06455
Alloy C-4 is a nickel-chromium-molybdenum alloy with outstanding high temperature stability.
CALL US:
1-866-725-8609Alloy C-4 is a nickel-chromium-molybdenum alloy with outstanding high temperature stability.
Alloy C-4 is a nickel-chromium-molybdenum alloy with outstanding high temperature stability. This alloy resists the formation of grain-boundary precipitates in the weld heat-affected zone, thus making it suitable for most chemical process applications in the as-welded condition. Alloy C-4 alloy also has excellent resistance to stress-corrosion cracking and to oxidizing atmospheres up to 1900°F (1038°C).
Components used in wastewater treatment
Components used in chemical processing
Nuclear fuel processing
Nickel: Balance
Chromium:14.00-18.00
Molybdenum: 14.00-17.00
Iron: 3.00 max
Cobalt: 2.00 max
Manganese: 1.00 max
Carbon: 0.015 max
Silicon: 0.08 max
Phosphorus: 0.04 max
Sulfur: 0.03 max
Titanium: 0.70 max
Density: 0.312 lb/in³, 8.64 g/cm³
Electrical Resistivity: micro-ohm-in, (micro-ohm-m):
At 74°F (23°C): 49.1(1.25)
At 212°F (100°C): 49.3 (1.25)
At 392°F (200°C): 49.6 (1.26)
At 572°F (300°C): 49.9 (1.27)
At 752°F (400°C): 50.2 (1.28)
At 932°F (500°C): 50.8 (1.29)
At 1112°F (600°C): 51.8 (1.32)
Specific Heat: BTU/lb-°F (J/Kg-K)
At 32°F (0°C): 97 (406)
At 212°F (100°C): 102 (427)
At 392°F (200°C): 107 (448)
At 572°F (300°C): 111 (465)
At 752°F (400°C): 114 (477)
At 932°F (400°C): 117 (490)
At 1112°F (500°C): 120 (502)
Thermal Conductivity: BTU-in/hr-ft²-°F (W/m•K)
At 74°F (23°C):70(10.1)
At 212°F (100°C):79 (11.4)
At 392°F (200°C):92 (13.2)
At 572°F (300°C):104 (15.0)
At 752°F (400°C):116 (16.7)
At 932°F (500°C):128 (18.4)
At 1112°F (600°C):142 (20.5)
Mean Coefficient of Thermal Expansion: µin/in-°F, (m/m-K)
68-200°F (20-93°C): 6.0 (10.8 x 10 )
68-400°F (20-204°C): 6.6 (11.9 x 10 )
68-600°F (20-316°C): 7.0 (12.6 x 10 )
68-800°F (20-427°C): 7.2 (13.0 x 10 )
68-1000°F (20-538°C): 7.4 (13.3 x 10 )
68-1200°F (20-649°C): 7.5 (13.5 x 10 )
68-1400°F (20-760°C): 8.0 (14.4 x 10 )
68-1600°F (20-871°C): 8.3 (14.9 x 10 )
68-1800°F (20-982°C): 8.7 (15.7 x 10 )
Modulus of Elasticity: KSI (MPa)
30.8 x 10³(211 x 10³) in tension
Melting Point: 2550°F (1399°C):
Ultimate Tensile Strength: 100 KSI min (690 MPa min)
Yield Strength: 40 KSI min (276 MPa min)
Elongation: 40% min
Hardness: Rb 100 max (aim)
Alloy C-4can be cold rolled to achieve the temper properties required by specific customers and/or manufacturing requirements. Contact Ulbrich Wire for details.
Refer to NACE (National Association of Corrosion Engineers) for recommendations.
Alloy C-4 is non-hardenable by heat treatment.
For best results refer to: SSINA’s “Welding of Stainless Steels and Other Joining Methods”.
Hastelloy® C-4 is a registered trademark of Haynes International
Limitation of Liability and Disclaimer of Warranty: In no event will Ulbrich Stainless Steels and Special Metals, Inc., be liable for any damages arising from the use of the information included in this document or that it is suitable for the ‘applications’ noted. We believe the information and data provided to be accurate to the best of our knowledge but, all data is
considered typical values only. It is intended for reference and general information and not recommended for specification, design or engineering purposes. Ulbrich assumes no implied or express warranty in regard to the creation or accuracy of the data provided in this document.
Thanks for your interest in Ulbrich! Whether you're developing a new product or ramping up production, we'll be happy to learn more about your specific needs. Please fill out the form below, and we will promptly get back to you with a quote or, if needed, a request for more information.